Sample VT400 °C exhibits a more uniform particle measurement distribution and pores with a mean grain measurement of about 12 nm (In line with ImageJ software program Examination). However, changing deposition temperature to 700 °C larger sized and denser particles with a median grain sizing of 460 nm was acquired. Sample VT400 on the other h